Chemical Composition
0.05 to 15
%    
0.003
%    
0.03
%  (maximum)  
7 to 8.5
%    
51.8 to 71
%    (estimate)
4.6 to 5.2
%    
17 to 19
%    
0.3 to 0.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
3.34e7
lbf/ft^2    
3.51e7
lbf/ft^2    
12
% strain    
 
Other Information
Maraged: 243,000 TS; 232,000 YS; 12 El; 57 RA; 48 HRC; For fuel rocket cases, aircraft landing gears, missile and aircraft components. Maraging steel, high strength, ductility and toughness.