Chemical Composition
0.45
%  (maximum)  
0.95
%    
97.6 to 98.1
%    (estimate)
0.8
%    
0.2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
414 to 965
MPa    
621 to 1140
MPa    
9 to 20
% strain    
240 to 310
   
 