Range attributes
0.1
%    
0.02
%    
9.8
%    
66
%    (estimate)
0.06
%    
4.8
%    
18.2
%    
0.06
%    
1
%    
 
Logical attributes
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
For bare welding wire; maraging steel grade 250, for submerged arc welding.
NIMAR 701
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For bare welding wire; maraging steel grade 250, for submerged arc welding.
 