Chemical Composition
0.03 to 0.07
%    
16 to 18.5
%    
61.9 to 71.5
%    (estimate)
2
%  (maximum)  
2 to 2.5
%    
10.5 to 14
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 