Chemical Composition
0.02
%  (minimum)  
0.24
%  (maximum)  
97.5 to 100
%    (estimate)
1.6
%  (maximum)  
0.009
%  (maximum)  
0.045
%  (maximum)  
0.045
%  (maximum)  
0.55
%  (maximum)  
 



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®