Range attributes
0.15
%  (maximum)  
17 to 19
%    
67.5 to 74.9
%    (estimate)
2
%  (maximum)  
8 to 10
%    
0.15 to 0.35
%    
1
%  (maximum)  
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Germany
Free-machining austenitic stainless steel, for screw machined parts. WNr. 1.4305. AISI 303.
AMBO NR 2 AZ
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Free-machining austenitic stainless steel, for screw machined parts. WNr. 1.4305. AISI 303.
 
Hyperlink attributes
Integer attributes
ID
64664
232016
 
Further Information



No warranty is given for the accuracy of these data