Chemical Composition
0.12
%  (maximum)  
16 to 18
%    
69.9 to 77
%    (estimate)
2
%  (maximum)  
7 to 9
%    
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 