Range attributes
180
   
0.22
%    
17
%    
30
% strain    
81.3
%    (estimate)
1.5
%    
345
MPa    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Germany
Annealed: 85,000 TS; 50,000 YS; 30 El; 55 RA; 180 HB; For furnace parts, grids, conveyors; corrosion and heat resistant.
NICROMA 17
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Annealed: 85,000 TS; 50,000 YS; 30 El; 55 RA; 180 HB; For furnace parts, grids, conveyors; corrosion and heat resistant.
 
Hyperlink attributes
Integer attributes
ID
64778
232016
 
Further Information



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®