Chemical Composition
0.12
%    
16.5
%    
82.9
%    (estimate)
0.25
%    
0.2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
345
MPa    
25
% strain    
150
   
 
Other Information