Range attributes
0.42
%    
1
%    
97.7
%    (estimate)
0.65
%    
0.2
%    
 
Logical attributes
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Germany
For gears, studs, bolts, shafts; oil hardened, tough.
AMBO CMV30
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For gears, studs, bolts, shafts; oil hardened, tough.
 