Chemical Composition
1
%    
0.09
%    
30
%    (estimate)
0.8
%    
65.5
%    
0.08
%    
2.5
%    
Cu is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Links
Organizations

 



No warranty is given for the accuracy of these data