Range attributes
1
%    
5
%    
92.7
%    (estimate)
1
%    
58 to 62
   
0.3
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Usually at 58-62 HRC; General purpose air hardening cold work die steel; good wear resistance and toughness. For blanking and forming dies, punches, rolls and trim dies. AISI A2.
SAGAMORE
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Usually at 58-62 HRC; General purpose air hardening cold work die steel; good wear resistance and toughness. For blanking and forming dies, punches, rolls and trim dies. AISI A2.
 